Results 1 to 1 of 1
  1. #1
    kunal is offline Junior Member
    Join Date
    Aug 2010
    Posts
    1

    Default Window lamination Problem.

    We are facing problem of shrinkage of film in corners of the window of our carton whose gsm is 296 . We have tried using 12 micron BOPP film, 12 micron Polyester film but still no gr8 result. also there is a possibility of some problem in our glue . Please help....