Search results

  1. I

    UV vs Conventional Printing

    I would like to chime in here, after reading these posts. I am very familiar with the product line that is being discussed, and I know who is using it. I also know that it does exactly what Print Pro says, without fault. "A Better Way" however, should not make comments like the one he made ever...
  2. I

    Opinions on Van Son Ink

    Ender - I am not sure if you were drunk when you wrote this un-decipherable note that you left for me?. You are probably some sort of Gans employee that is trying desperatly to defend the company's decision, you are not helping. Either way, you sound like you wouldnt understand how business...
  3. I

    Opinions on Van Son Ink

    I am not sure how comparing a large, worldwide ink company that manufactures in Asia and other countries to support its worldwide sales compares to a small Gans ink that simply went to China to get cheaper products to sell in its small American market. A.sures, you are making your company look...
  4. I

    UV Gloss Varnish Turning Black areas Dull?

    switch to a slower drying, stronger black. Despite common logic (as stated in other replies) it is the opposite of what they think. Let me know if you cannot solve this common issue.
  5. I

    Opinions on Van Son Ink

    I thought Gans brought most of their sheetfed ink in from China these days - dont tell me they dont. And didnt Braden get bought by Sun Chem? - in the end cheap ink is cheaper - cheaper materials produce ink with weaker film and poor drying, especialy in poor conditions. Aqueous coating has made...
  6. I

    problem with carbonization

    Bob Peterson is correct. The Hostmann Resista however, is a hard dry type ink that sets slow, but is designed to dry on hard to cure substrates. I am sure they have faster setting lines to offer, if the issue is the ink.
  7. I

    silver chalking

    I asked if you were on board stock because it has a particular effect on metallic inks, especially silver. The heavier the board, the worse this issue usually is. It is caused by the soft vehicle needed to carry the metallic particles diving into the board, leaving a thin layer of metal particle...
  8. I

    FDA Approved UV Gloss coating

    Hi Joe - would there be direct food contact?
  9. I

    Printing "raised ink"?

    we do it with a "raising varnish" - cured by UV, it does want to take two passes though.
  10. I

    silver chalking

    are you printing on a board stock?

PressWise

A 30-day Fix for Managed Chaos

As any print professional knows, printing can be managed chaos. Software that solves multiple problems and provides measurable and monetizable value has a direct impact on the bottom-line.

“We reduced order entry costs by about 40%.” Significant savings in a shop that turns about 500 jobs a month.


Learn how…….

 
Back
Top