Is scuffing and scratching the nature of the soft aqueous coating no matter how long it dries? We have gone back to printed sheets from February 2010 and the coating does scuff and scratch although not as bad as first as coming off press. We run a Komori LS-40 6/c with coater and have been using Nicoat Soft Aqueous coating. The anilox roller has a 10.3 bcm if this helps. Any suggestions would be appreciated. Thanks!
Is scuffing and scratching the nature of the soft aqueous coating no matter how long it dries? We have gone back to printed sheets from February 2010 and the coating does scuff and scratch although not as bad as first as coming off press. We run a Komori LS-40 6/c with coater and have been using Nicoat Soft Aqueous coating. The anilox roller has a 10.3 bcm if this helps. Any suggestions would be appreciated. Thanks!