Currently we are getting some coating build up on the tail edge of the sheet (in the spot where the packing drops off) on our Lithrone 28 with 3 roller Komori Coater (Steel pan roller, rubber metering and steel aplicator roller). This isn't usually a problem, but we have a very large run of 80# Text Gloss, and it can cause the sheets to stick together if we don't shut down to clean the coater blanket at regular intervals.
-Checked blanket and packing thickeness
-Packing is cut sharply and cleanly
-Blanket to impression set at "kiss" nip squeeze
-Adjusted aplicator roller to 5mm squeeze to blanket, which is the setting the maual has listed
-Adjusted aplicator roller to 4mm (just in case)
-Checked coating viscosity
-Tried reducing coating feed drastically
Any comments or suggestions as to something else I could try? Thanks,
K
Currently we are getting some coating build up on the tail edge of the sheet (in the spot where the packing drops off) on our Lithrone 28 with 3 roller Komori Coater (Steel pan roller, rubber metering and steel aplicator roller). This isn't usually a problem, but we have a very large run of 80# Text Gloss, and it can cause the sheets to stick together if we don't shut down to clean the coater blanket at regular intervals.
-Checked blanket and packing thickeness
-Packing is cut sharply and cleanly
-Blanket to impression set at "kiss" nip squeeze
-Adjusted aplicator roller to 5mm squeeze to blanket, which is the setting the maual has listed
-Adjusted aplicator roller to 4mm (just in case)
-Checked coating viscosity
-Tried reducing coating feed drastically
Any comments or suggestions as to something else I could try? Thanks,