aqazi81,
You misunderstand my comment "try printing just with H2O" NO you cannot print just with water in the long run,
Chem- free/ DoP plates do not have the necessary "Desensitized Layer" this layer "One micron thick" NEEDS to be
Induced on the plate during the Image development step.
The only plates that ran successfully with just H2O were "Deep Etch Plates" then only a max. of 10.000/20.000 sheets
before Scumming appeared,
Remmember aqazi81,
It is all about maintaining the Diffferent Inter- Facial Tensions on the on the - Induced Layers - 1) Hydrophillic 2) Oleophilllic
Regards, Alois