How do you people deal with drying on vinyl material in sheetfed offset?
Chemistry is set to match the material and ink specifications, also fast drying inks are used.
Small stacks are used during printing, climate within the production room is fine. Actually, everything seems to be fine.
Still, it happened for second time that the stock wouldn't drie even after 3 days.
At the end, we applied waterbased coating on the stock, and the problem was solved.
Chemistry is set to match the material and ink specifications, also fast drying inks are used.
Small stacks are used during printing, climate within the production room is fine. Actually, everything seems to be fine.
Still, it happened for second time that the stock wouldn't drie even after 3 days.
At the end, we applied waterbased coating on the stock, and the problem was solved.