ANDERSON 1958
Member
When finishing for example a 24 pp a5 booklet 300 gsm cover 150 gsm text we are getting cracking down the spine, finished om a morgana. Also for example when cutting 400 gsm business cards the cards split around the outside even with a new blade.
Using different stocks will sort the problem but am sure you guys will have fix. I have been told a higher or lower temperature will sort the problems but so far this has not worked.
Also uk operators what silk stock are you using as suppliers at the moment seem to be running out very quickly..The Brexit effect perhaps.
Using different stocks will sort the problem but am sure you guys will have fix. I have been told a higher or lower temperature will sort the problems but so far this has not worked.
Also uk operators what silk stock are you using as suppliers at the moment seem to be running out very quickly..The Brexit effect perhaps.