WI-Flexo
Well-known member
As the title states, looking for anyone with experience printing shrink film on a MA-P7 with water based ink. We are having a problem with ink drying WAY to fast on the plate (Dupont DFM and DFR). We have tried two different ink systems with very similar results. Ink techs are at a loss but are thinking may be press related (residual heat, possibly airflow around cylinders, or some other unknown).
ANY insight greatly appreciated!!
Thanks.
ANY insight greatly appreciated!!
Thanks.